According to the above mathematical model, it can calculate final ferritegrainsize after rolling cooling.
按照上述给出的数学模型,可计算出轧制冷却后最终的铁素体晶粒的大小。
2
Different ferritegrainsize and combination of ferrite, bainite and martensite phases were obtained according to the control of cooling rate.
通过冷却速度的控制实现钢材内部铁素体、贝氏体、马氏体不同的相组成和铁素体晶粒尺寸。
3
In this study, the effects of plasticdeformation of the austenite phase and the holding temperature on thetransformation kinetics and the ferritegrainsize are investigated.