... 硬化层深度|case depth 硬化层深度|depth of hardened layer 硬化电路|hardened circuit ...
双语例句
1
The depthofhardenedlayer after surface quenching was about 0.
磨 辊 齿经等离子弧表面淬火后硬化层的厚度约为0。
2
Compared with the dry-grinding, the surface compress residual stresses of the hardenedlayer under wet-grinding is increased, but its depthofhardenedlayer reduces about 30%.
与干磨相比,湿磨硬化层表面残余压应力有所提高,但其硬化层深度减少了约30%。
3
This paper demonstrates residual stress of induction quench parts and personal views about stress distribution of flange corner heat treatment, truck half axle material and depthofhardenedlayer.