Investigation was made of effect of preplastic deformation for unexplosive and explosive treatments on strength, surface residual stress and hydrogen embrittlement of the specimens.
研究了预塑变对爆轰处理和未爆轰处理样品的强度、表面残留应力、氢脆敏感性及其关系的影响。
2
Soldering on ADI surface decreased the ADI tensile strength and elongation, and solder coating could not prevent from water embrittlement.
试样表面镀锡使ADI的抗拉强度和伸长率下降,镀锡层不能有效防止ADI的水脆化。
3
Rust against heat-treated water-embrittlement resistance to further develop the ultra-thin thickness of chromic acid-high corrosion resistance of the surface treatment technology.