The higher initial strainhardening rate and higher strength of dual phase are attributed to rapid strainhardening in ferrite and the load transfer from the ferrite to martensite.
铁素体迅速应变硬化和铁素体到马氏体的载荷传递使双相钢具有较高的初始应变硬化速率和较高的强度。
2
With the strain aging temperature increasing, strength and hardness increases, plasticity and toughness decreases, yield ratio has the ascending trend, hardening index decreases.
随着应变时效温度升高,强度和硬度增加,塑性和韧性下降,屈强比呈升高的趋势,形变强化指数降低。
3
Compared with the strip produced by conventional austenite rolling, the yield strength of the ferrite rolled strip was lower by about 20%, with same elongation and strainhardening exponent.