The initial attack has the characteristics of localized corrosion.
镁合金的初期腐蚀具有局部腐蚀的特征。
2
The exposure used in this practice is not intended to simulate the deterioration caused by localized weather phenomena such as atmospheric pollution, biological attack, and saltwater exposure.
本标准使用的老化条件并不试图去模拟当地气候现象如大气污染、生物侵蚀,以及盐水老化导致的性能退化。
3
Almost any lack of homogeneity of the metal surface or its environment may initiate attack, by causing a difference in potential. The result is corrosion that is usually localized.