The hydration energy increased gradually and obtained a saturated value at the end.
水合能逐渐升高并最终趋于平衡,平衡值仍低于体相水的势能。
2
The results show that the early strength and the permeability of concrete can be improved effectively, and the hydration heat can be reduced and the hot peak value at the early age can be postponed.