Bitumen modification: The low temperature flexing and anti-flowing property at high temperature of bitumen can be improved by adding 3% to 15% (wt %) SBS.
沥青改性:在沥青中加入3%—15%的SBS可改善沥青的低温屈挠性和高温抗流动性能。