Under the optimum technology condition, we can get the anhydrous scandium chloride molten salt whose hydrolysis rate is2.3%.
在此工艺条件下,制得的无水氯化钪熔盐中钪的水解率为2.3%。
2
Oxidizing agent was prepared by means of anhydrous manganous acetate dissolved in glacial acetic acid and oxidized to divalent manganic salt by potassium permanganate.