The results show that producing HRB400 reinforced bar can substitute low alloy for conventional V microalloy process by composition adjusting and rational cooling control after rolling.
The results showed that: the amounts of releasing ions per second, Al-V-Ti alloy was the least, followed by 3 kinds of stainless steel, Ni-Cr alloy, Cu alloy.
结果显示:每秒钟释放的离子数,以铝钒钛合金最少,3种不锈钢次之,镍铬合金较多,铜合金最多。
3
The results show that the wear resistance can be improved by using fine particle, even and high content of V in the alloy.