The optimal formula of the UV curable conductive adhesive gained from single factor test was as follows: Silver-plated copper powder 70%, complex photoinitiator 4%, AIBN 2% and KH570 2.5%.
The measures of improving locomotive structural design and electric compensation may be taken to raise the utilization factor of adhesive weight of electric locomotives above 94%.
采用机车的结构设计及电气补偿两项措施,可使电力机车的粘着重量利用率增至94%以上。
3
Methods Taking raw material of formula as factor and adhesive force as marker, orthogonal test was used to optimize the matrix ratio in cataplasm.