The dissolution was confirmed to be a quasi-reversible process, which was controlled by solid-statediffusion and charge transfer.
证明针镍矿的阳极溶解是由固相内扩散传质和电荷传递步骤混合控制的准可逆电极过程;
2
Cycling life tests investigated that the capacity of alloy prepared by ball milling decreased to 40% after 50 cycles, while the solid-statediffusion method just 25 cycles.
The variation of the carbon diffusion coefficient at the vicinity of the phase boundary during the process of eutectic solidstate phase transformation of the phase boundary was analyzed.