The effect of the reaction conditions on reaction rate and final productparticle size was also studied.
同时考察了反应条件对反应速度、最终产品粒度的影响。
2
Due to the improvement of the structure of productparticle size, the result of reverse flotation was greatly improved, with the metal recovery increasing from 68. 65% to 74. 07%.