The results showed that the burst failure of the primary cyclone separator was caused by inadequate material strength resulted from flushing damage and reduced in thickness in large area.
结果表明,一级旋风分离器爆裂是由于其下封头受到冲蚀损伤,壁厚大面积减薄导致材料强度不足所致。