环境科学技术 制备 The results showed that the suitable experimental condition of preparing exfoliated graphite was m1 (nature flake graphite):m2 (perchloric acid):m3 (potassium permanganate)= 1:4:0.5, reaction temperature was 35℃, reaction time was 40 min. 结果表明:膨胀石墨制备的最佳实验条件为m1(天然鳞片石墨):m2(高氯酸):m3(高锰酸钾)=1:4:0.5,反应温度为35℃,反应时间为40 min。