The result shows that under the optimal conditions, the content of double carbon bond in product reduced, and the comprehensive properties, especially, the oxidative resistance improved greatly.
结果表明:在此条件下加氢,产物碳碳双键含量减少,其综合性能特别是高温耐氧化性得到了显著提高。
2
Bending strength, compressive strength, interfacial bond strength and frost-resistance were also studied and analyzed.
并对其抗压、抗折、新老界面粘结强度及抗冻性等进行了实验研究。
3
The material had high emissivity, high bond strength and thermal shock resistance, it was a mew ceramic material of high efficiency and saving energy.