This article deals with the kinetics of thermal decomposition process of non-coking coal with modified coal tar pitch used in a steel company.
本文对国内某钢铁公司焦化厂所用的非焦煤配改质沥青的分解过程进行了动力学研究。
2
The plastometer thickness of No. 2 coking coal and 1/3 coking coal increased dramatically by adding modified coal tar pitch, meanwhile, the coal caking indexes increased dramatically.
随着改质沥青的加入,焦2煤和1/3焦煤的胶质层厚度显著增加,焦2煤的粘结性指数也显著增加。
3
Maintaining basically same quality of coke, the mixing of medium temperature pitch can appropriately reduce the mixed volume of high quality coking coal and fat coal, decrease the cost of mixed coal.