The film thickness shows about 8% variation for the whole annealingrange.
在整个退火区域,膜厚度有大约8%变化。
2
The secondary recrystallization and its temperature range of grain oriented silicon steel have been studied by the method of interrupting secondary recrystallization annealing.
采用"中断法"研究了取向硅钢二次再结晶过程中的异常长大行为,确定了二次再结晶发生的温度范围。
3
In box annealing a ferrous alloy, the charge is usually heated slowly to a temperature below the transformation range, but sometimes above or within it, and is then cooled slowly.