The formation of "black layer" is also controlled by the nitrogenpotential and system temperature in the deposition chamber.
同时,“黑色层”能否形成还与气氛氮势、体系温度有关。
2
Higher nitrogenpotential may promote formation of white layer, increase hardness and wear resistance but at the same time increase brittleness of nitriding case.
提高氮势可促使白层形成,提高渗层硬度和耐磨性,但使其脆性增高。