When joint is filled, a continuous run of solder or brazing alloy will be visible.
在安装连接部件时,可以看到焊料和钎焊合金继续流动。
2
This paper discusses the effect of brazing time, brazing temperature, brazing gap and diffusion treatment on the remelt temperature of the brazed joint.
文章讨论了钎焊时间、钎焊温度、钎焊间隙及焊后扩散处理对钎焊接头再熔化温度的影响。
3
To make a proper brazingjoint, the clearance between the solder cup and the tube should be approximately 0.001" to 0.010" (0.0254mm to 0.254mm).