The hardening case depth and hardnesscurve can be changed by adjusting heating time, heating power and cooling speed during induction hardening.
在感应淬火中,通过改变加热时间、加热功率和冷却速度可以改变淬硬层深度和硬度梯度。
2
According to the tempering temperature and hardnesscurve, the redistribution of residual stress is associated with the transformation of residual austenite.
由回火温度与硬度变化曲线证实,残余应力重新分布是与残余奥氏体转变相关联。
3
The hardness of the alloy following the change of time was analyzed by micro- hardness instrument and the alloy's hardnesscurve following the change of time was drawn.