The factors controlling the amount of (?)FeO in the finalslag is discussed.
讨论了控制终渣氧化铁含量之因素。
2
The effective preventing measures are improving the fluidity of finalslag and separation of slag from hot metal.
改善高炉终渣的粘度温度性能,提高渣、铁分离能力是防治产生铁沟沉积物的有效措施。
3
In finalslag, the content of tricalcium silicate increase 60%, the content of calcium ferrite decrease 25%, the microstructure turn from granular into interweave structure.