XRD results indicate that amorphous titanium oxidefilm is formed on the surface after anodic oxidation, and corrosion rates of titanium crystal vary along different crystalline orientation.
In particular, the amorphous titanium oxide is obtained by using the reactive sputtering method and via deposition at a low temperature and at a high film formation rate.